Try starting off at 30 amps, I would use a large gas shield with a diffuser and move slowly as you want the cooling pool of weld well protected, if welding pipe back purge the work piece fill with argon or nitrogen at 3 lpm remember and leve a vent hole the far side so as not to cause any internal pressure which can blow out. If the weld is turning white when cooling you are moving too fast or dont have enough shield gas covering the pool , you are looking for a nice cobalt blue colour on the finished weld. Thats in my limited experiance on welding titanium.