TIG Welding Help

Balls...
I can't play the Guitar either... I was really hoping to get half good at welding, as I spent most of my life soldering and Brazing.
Brazing is almost oxy/acetylene which is kind of analogous to TIG so your half way there 👍
 
Shown the welder in work, he hasn't read any replies.

Flow should be 4-6 for welding inside. Extra for outside.

He said to look for pinprick holes in your Argon line. Gas wont escape but will draw air in. Contaminating the gas.

Hold your torch over weld when finished, or increase post flow time if needed.

Make sure parts are fully degreased and clean.

Make sure tip is sharp, regrind if dipped in pool.

Grind point inline with tungsten, not radially

Arc length is too long. Get tip closer to work, to avoid undercutting.
 
He was using the esab caddy we have
20210104_143119.webp
20210104_143549.webp
 
I’m a retired welder with years of experience welding aluminum for a subsea ROV company. If you are wanting to weld aluminium i don’t think you have the machine to do it , is it an AC machine with Ac balance control? i always use a lathanated tungsten with balled end ,a argon helium mix gas, but pure argon is fine for thin material , if it is thicker you have to preheat . Aluminium must be clean before welding ,the surface of aluminium is always oxidised use a stainless steel brush to clean . Hope this of use to you .happy if you need any advice.
 
I’m a retired welder with years of experience welding aluminum for a subsea ROV company. If you are wanting to weld aluminium i don’t think you have the machine to do it , is it an AC machine with Ac balance control? i always use a lathanated tungsten with balled end ,a argon helium mix gas, but pure argon is fine for thin material , if it is thicker you have to preheat . Aluminium must be clean before welding ,the surface of aluminium is always oxidised use a stainless steel brush to clean . Hope this of use to you .happy if you need any advice.
He isn't welding aluminium.
 
Practice practice practice, Noods mentions starting with a lower amperage, this can be counter productive as a lower amperage means you are holding the torch on the material longer hence building up heat throughout the material before it's started to melt particularly with alloy, it's natural for beginners to use too low an amperage because we are frightened of blowing holes in the material and we cant run the bead fast enough but it doesn't always work that way. I never stop practicing and making fine adjustments and taking notes of my findings.
Steve
With respect Steve that’s not quite what i was trying to say with regards to starting at a lower amperage .. Lost in post i’m sure but what i was trying to portray was rather than go in with a suggested figure of 100amps on a piece and finding things getting a little out of control very quickly eg holes etc try going in at say 90amps ( if no foot pedal) and gain more control with things while your learning, yes i agree by staying put for too long will bring distortion issues etc but, if the learner finds his not forming a puddle quick enough etc it’s better, to increase his amps by say 5 amps at a time than having to go the other way eg have no control and having to decrease amps after already producing a mess, eg better for learning and confidence overall.. Cleanliness and control along with clamping ( clamp your work down on the bench to lessen distortion) are key to confidence and visible progress.. IMO.. X
 
I got a taste of Scratch start when I did my course, but moved on to the pedal quickly.
I'm sure I'll have to use it at some stage, laying under a car for example pretty much stops you using a pedal.

Nasher.
 
I got a taste of Scratch start when I did my course, but moved on to the pedal quickly.
I'm sure I'll have to use it at some stage, laying under a car for example pretty much stops you using a pedal
Nope ... you put the pedal between your knees/ thighs and squeeze
 
Back