fileing welds flat

Scotty

New member
a bit like this,

ive convinced myslef it just practice

was thinking just perhaps if i get my frame repainted i might want to smooth the frame welds first

or is that a realy stupid idea :confused:
 
why though ? shurly the buldge over and above the lowest part is just excess metal and the 'weak point' as it were is where the metal is thinest at the trough as it were
 
one of the reason i always favoured Cannondale mtb frames and Koga road cycle frames was the finish on the frames, all welds filed flat. Attention to detail. As long as it is the excess material you are filing away and not the structural stuff I don't see any probs. then again im no expert on the matter but it looks great when done
 
one of the reason i always favoured Cannondale mtb frames and Koga road cycle frames was the finish on the frames, all welds filed flat. Attention to detail. As long as it is the excess material you are filing away and not the structural stuff I don't see any probs. then again im no expert on the matter but it looks great when done

Cannondale and Klein they always looked the best bikes with the frame welds, attention to detail was everything but they were big welds filed back not small I guess???

http://mag1.olivesoftware.com/Activ...ction=TKM_AM&ReaderStyle=Normal&OnePageMode=1
 
you can file them down and not do any harm so long as you dont go too far. my old man was a welder to trade and always finished his welds off by taking an angle grinder to them and you couldnt tell it had been welded when he was finished.
it might be an idea to try welding a few bits and pieces together and practice grinding them down so you know how it goes. if the welds are any good there will be no need for filler when you grind them down
 
a bit like this,

ive convinced myslef it just practice

was thinking just perhaps if i get my frame repainted i might want to smooth the frame welds first

or is that a realy stupid idea :confused:

...this looks like an exhaust piece whereby one bit fits into the other then welded. Why do you want to do this anyway mate? :)
 
The weld 'bulge' is the excess metal melted into the join with the welding rod. (talking about arc welding). It was my understanding that the purpose of the weld was to melt the adjoining pieces of metal and to mix the particles toegether so as to form an indiscernable piece of metal - although this would never be achievable.
Site welders have a certificate stamp that they put next to every weld so when the weld is x-rayed the welder can be retested if the weld is poor.
Grinding the bulge down will obviously reduce the value of the weld but at the same time the strength should remain.
 
If its a fillet weld don't file too much as the weld depends on its throat thickness for strength. If it's a partial penetration butt weld again be careful. If it's a full penetration butt weld you can file until smooth and in-line with the adjoining pieces. That's my understanding of structural welds.
 